1

Topic: Printing accuracy questions - newbie

Hello i do own a Da vinci 2.0A and i have some newbie questions

Should i install reqetier firmware ? smile

About accuracy (for small items) , while you can choose layer height (0.1-0.4)  each dot's radius is 0.4mm ? (nozzle radius)

if i want to print a thin line i better put the object that way so the line printed horizontally (with 0.1 layer height) not not vertically ?
(i try to make some small stamps and i find some problems on that)

2

Re: Printing accuracy questions - newbie

my bed is 95,97,92 should i leave it this way or i better do it 100 100 100|?

3

Re: Printing accuracy questions - newbie

Repetier will give you greater accuracy, for sure.
Regarding auto calibration, forget it and use the manual method in the sticky section of this forum.

Davinci 1.0 with repetier firmware & E3D V6 Lite
Anycubic Photon DLP printer, Einscan-S 3D scanner
Simplify3d, 123D Design, Meshmixer
http://www.thingiverse.com/scobo/designs