1

Topic: weird extruding has me stumped

I am having inconsistent extrusion amounts during a print. I tried loosening the hob bolt and tightening it. I checked the bed leveling and it's fine. The only thing I didn't check for was a jam. But I just cleaned out a jam a few weeks ago so I find it hard to believe. Here is a picture of the printed lines.

Post's attachments

20151015_200316.jpg
20151015_200316.jpg 4.06 mb, 1 downloads since 2015-10-16 

You don't have the permssions to download the attachments of this post.

2

Re: weird extruding has me stumped

Your bed is not level, or your glass is warped. the lack of filament indicates an area that is too high while the more filament indicates a low area.  When you level a bed you should use a .25 or .20 feeler gauge. Start at one corner, work clockwise or counter clockwise then go back to the middle. And confirm it is level as well as the original corner. Each corner will offset the other three slightly so you have to make multiple passes.

If your bed is warped as it looks like it is then you have to try to reach a compromise between the high and low areas.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: weird extruding has me stumped

Hmm. I just had it leveled perfectly. I don't know what I did to mess up the leveling. I think my main problem is with the tension bolt spring and gear. The MK series come uncalibrated so spring tension is weak. which requires adding more tension to get the gear against the idler wheel. I am trying to adjust it again since I think the spring lost some tension over the year. Right now the filament can be pulled out easily when the extruder is idle, but when extruding its harder to pull out the filament but I still can. If I add too much tension the extruder skips and clicks.

4

Re: weird extruding has me stumped

Two other things to check. Your hot end may be too close to the bed. It will restrict output. The other, it looks like a partial clog to me. It extrudes, but not well. Use a cold pull method to clean out the hot end. Search for it if you have not seen it before.

SD2 Expert stock, ABS fume fan,
XYZ DaVinci 1.0 stock ABS, Simplify3D
QUBD Two-Up PLA, new 3D printed X gantry, Y idler, flex z coupler, extruder mount, E3D Lite

5

Re: weird extruding has me stumped

Thanks, I'll give it a try. Does pla work for cold pull method? I read that nylon is recommended.

6

Re: weird extruding has me stumped

Often for pla that is what you have to do as you cant dissolve it. that or pull it out and torch it

7

Re: weird extruding has me stumped

PLA will work with cold pull, let it cool to around 80c and it should work.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

8

Re: weird extruding has me stumped

Well I leveled the bed and cleared the nozzle and was printing great for a good hour until I reached the finer detail part of the print and it stopped extruding and I came back to it moving over the print with nothing extruding. Could this have to do with my retraction settings? It's set at 3.4mm and it was doing a lot of retracting. Gas I hate having these weird problems. Here is a picture of the failed print.http://soliforum.com/i/?EfsipBz.jpg

9

Re: weird extruding has me stumped

I think my temp was too high and retraction too high to cause these problems. I'm going to try again one more time tomorrow. Can't really waste pla steel with these large prints.

10

Re: weird extruding has me stumped

I also recommend using vegetable oil with PLA it helps a lot.

11

Re: weird extruding has me stumped

Of course you have to always watch out for the swelling when the PLA heats up.  You can move the fan down a bit to cool the neck of the hotend, so the heat won't creep as much.
Works for me.

Da Vinci 2.0 with Repetier Firmware (Printing in ABS/PLA/Exotics)
12 Years PC Experience
16 years old

12

Re: weird extruding has me stumped

It was bed leveling and retraction.