Topic: Post-Extrusion Water Bath
All industrial filament extrusion machines seem to have water baths. Obviously, filastruder doesn't. Beyond complexity, is there a reason? Is it simply unnecessary? Filastruder seems to get tolerances similar to commercial filament, so is the water bath actually doing something else?