Topic: Wanhao ABS Filament Any Help?
I re-flashed my 1.0a to repertier so I could use third party filaments and have lots of other stuff. It was fairly easy and I had no problems doing it (I am quite experienced with tech but a newbie to 3d printing).
When I print with da vinci filament at a bed temp of 90 and an extruder temp of 212 every thing comes out great. I even printed this https://www.thingiverse.com/make:157917 and it came out perfectly and fully working(I have spent some time dialing the printer in)
However when I tried some Wanhao gray and gold ABS filament things turn to poo. The edges curl up and the top layer is just goop. I have tried every temperature range from a bed of 90 to 120 and an extruder temperature of 200 to 240 (which baked in the there and I spent an hour drilling it get the bloody stuff out.) and just about every combination of the two. It isn't an issues of the filament not sticking to the bed. The first few layers stick fine to the glue but after 4 or 5 layers it stars curling up at the sides. The bottom layers don't curl up just the layers above layer 4 or 5.
I have been testing this with a 20x20x20 cube. When I print something bigger it is a little better but not much.
Is it just bad filament or is the da vinci stuff just really good and easy to use? Any help would be appreciated, thanks.