Topic: da Vinci 1.1 Plus - camera
Greetings all
I was curious if anyone has info on the camera, specifically the URL streams, anything like http or rtsp streams that I can access directly? Perhaps a simple mod to get to the camera stream? The XYZ app allows you to see the camera so it's the stream is available somehow?
background:
I just purchased this printer and loving it. I've already done the arduino cartridge mod and works great. I am to use other ABS filaments. Now I am experimenting with PLA. I am able to print using XYZ PLA just fine, but I am getting inconsistent prints with third party PLAs. I'm trying different temp settings, seems to work here and there. Mostly, must have raft turned on to get a good print, likely due to low bed temp. more to come.
thanks in advance