Topic: xyz 1.0A filament not extruding
Hello,
I've recently bought a da vinci printer, i use a hacked cartidge and have been printing about 120 hours with ABS.
Last night, 3rd party cartidge got stuck on its stand, and broke. I tried to load the filament again but but could not.
Than, I took the extruder out and saw that broken part was below the extuder motors discs. So it couldn't push the broken part of the filament. I tried to take out the broken filament, while the nozzle is hot, but it did not work either. The filament broke again leaving a small piece in the canal going to nozzle.
I even tried pushing it manually with a piece of filament, of course when the nozzle is hot, it did not work either. I tried cleaning the nozlle with thinf wires that comes with it, it did not work.
What is the problem here ? How can i fix this?
Thanks for all the answer