Topic: Adding a z offset to stock xyzware?
Title is pretty self explanatory, is this this possible or do i need to physically offset the table lower using something thicker than paper to calibrate it lower?
I tried opening the code that the xyzware slicer generates but that was a non starter, any help appreciated.
Edit- to explain myself i get to much "smooshing" on the bottom few layers and i have been trying to print some thin items and they turn into fat ugly versions of themselves. Doesn't matter if i use ABS or PLA. Also i am using blue tape on my bed which adds a bit of height.