1 (edited by ysb 2013-01-22 01:16:17)

Topic: abs pellets from osprinting

i just receive the abs pellets that i bought from osprintingllc.com

no problem with custom for me ( quebec / canada)  .. i bought 24 lbs to test elmoret extruder, and there is no special surprise. the pellets are natural one, and they seems to be clean.

the pellets are very cheap but the shipping is not, so you need to buy a lot to be effective (more than 20 lbs for me.)
so a full total of 88$can for 24lbs natural pellets including shipping . it's near 11 standard spools of filament for the price of 2 or the price of 6 if i add the price of the filastruder..... i' m very happy of my order as an international buyer.
now, i'm waiting for my extruder... :-P

2

Re: abs pellets from osprinting

+1 For OSPrinting

They sent my order fast and they are very low cost.  Even included some extra plastic with my order.

SD2 with E3D, SD Press, Form 1+
Filastruder
NYLON (taulman): http://www.soliforum.com/topic/466/nylon/

3

Re: abs pellets from osprinting

ysb, I'm assuming you went with fedex? I'm surprised you didn't get hit with customs. I'll be ordering to Ontario, and I'm afraid of getting hit with customs D:

4 (edited by ysb 2013-04-20 20:21:57)

Re: abs pellets from osprinting

Seshan wrote:

ysb, I'm assuming you went with fedex? I'm surprised you didn't get hit with customs. I'll be ordering to Ontario, and I'm afraid of getting hit with customs D:

fedex??? are you mad? ? wink never use a transporter from USA if you don't want to be stolen... i use usps...  transform to post canada when crossing the borderline ...no tax.. no custom...

choose 'more carrier' on the webstore to get USPS

5 (edited by Seshan 2013-04-20 23:30:38)

Re: abs pellets from osprinting

Hmm, Maybe they've changed it, the most I can order is 16lb (8 bags) before the USPS option disappears. sad Which makes it $15 a KG. It's $110 after shipping.

6

Re: abs pellets from osprinting

Just got my pellets today and no duty problems. I just wish I could of ordered more with USPS. D: