I purchased some fire red Ninja flex, just had to try my hand at printing this stuff.
It's like wet spaghetti to feed but my Bowden setup handled it with ease.
Printed off 3 items including the iphone case and they turned out great.
Hotend temp was 238c and bed 20c or cold worked best.
I used S3D to slice and slowed the print speed down to 20mm per Ninja flex recommendation.
All other settings were what I use for ABS.
Like to know what settings others use for Ninja flex to get the best print?