Topic: Weird problem with Splic3r in RH compred to Soliprint
OK. I prefer RH. It is much more controllable, and actually saves my settings between sessions! Soliprint doesn't and is a bit too basic. However, when I slice objects in RH, it seems to miss parts of the model out. The same model in Soliprint slices absolutely fine!
Check out the pics below. The first one (with the purple angel) is the original model as loaded into RH. The second one (with the blue angel) is the version after slicing. Notice that the shoulders have disappeared, and the head is now floating in mid-air. If I slice the exact same file with Soliprint, the shoulders are fine. Result is that RH prints the model and leaves a gap before it prints the head, which then (obviously) collapses. Soliprint prints the full thing, complete with shoulders. Why does this happen (I've had it happen with other models too)? Both use Slic3r. But one works and one doesn't.
Please help!
Edit: Forgot to attach the pictures! Done it now.