Topic: davinci 1.0 PLA problem
hello
My 3D printer davinci 1.0 repetier firmware 3DP01
filament 1.75 ESUN PLA color brown, I tested with transparent filament I have the same thing?
the filament enters the extruder smoothly.
it comes out smoothly at first and then clic clic clic ???
please look problem https://youtu.be/aXief8wxBvI
thank you for reading me and find the solutions together !
firmware repetier