Topic: Davinci 1.0 - Heatbed seems to melt objects.
Dear forum,
I have a Davinci 1.0, and it seems to mess up the objects i print with it. The objects print fine once the first 2-3mm has been printed, but it is the base 2-3mm that form a problem:
There are several brown spots (burnmarks for the ABS i use, i'd assume). The sides become wider and the bottom solid (100% filled), so my guess is that it melted. Attached to this post are images showing this problem, and it is further defined in the document:
http://www.filedropper.com/myprinterfai … tcorrectly
I have no experience with 3d printers aside from the one i have now, and would like to hear your thoughts (and preferably solutions) about the problem.
Thanks in advance!