Topic: Filament Ratings - Brand / Head Temp / Bed Temp / Type

Didn't see a topic on what Brands everyone got working and the best settings ...If a topic already exists...sorry for the extra topic.

When programming cartridge chips it will save a lot of time. 

Example:
Tested on Davinci 1.0a:
XYZPrinting ABS Blue / 201C / 90C /ABS
XYZPrinting PLA Natural / 190c / 45c / PLA

Here was my First Non-XYZ filament:
Zen Toolworks Blue Glow In The Dark PLA  : AMAZON :http://www.amazon.com/gp/product/B00GWUC5R8

Tested on Davinci 1.0a
Zen Toolworks Glow in the Dark/ 200c / 70c / PLA

Others:
PLA(1,75mm 3D Factories ) on XYZ Davinci AiO 1.0 : Extruder 200 °C, Bed 60 °C, Print Speed : Slow, Layer 0,1 - 0,3

Blog Post: http://wditech.com/index.php/3d/12-zen- … e-dark-pla

Post's attachments

top.jpg 193.8 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
Lightwave 11 / DaVinci 1.0a
www.wditech.com
www.omsmedia.com

2

Re: Filament Ratings - Brand / Head Temp / Bed Temp / Type

OMSmedia wrote:

Didn't see a topic on what Brands everyone got working and the best settings ...If a topic already exists...sorry for the extra topic.

When programming cartridge chips and using a stock DaVinci it will save a lot of time.  Here was my First Non-XYZ filament:
Zen Toolworks Blue Glow In The Dark PLA  : AMAZON :http://www.amazon.com/gp/product/B00GWUC5R8


Zen Toolworks Glow in the Dark/ 200c / 70c / PLA




Blog Post: http://wditech.com/index.php/3d/12-zen- … e-dark-pla


You should also specify which Da Vinci you use as a 1.0 cannot use PLA.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Filament Ratings - Brand / Head Temp / Bed Temp / Type

says in his signature its a 1.0a

4 (edited by carl_m1968 2015-06-06 04:24:28)

Re: Filament Ratings - Brand / Head Temp / Bed Temp / Type

batmaster wrote:

says in his signature its a 1.0a

I see that now but like me very few pay attention to sigs. If they did I would not have 10 or so ask what I print on.

So back on topic it helps just to say it and avoid confusion. We still have users that think a 1.0 will print with PLA. It will not with out modding or buying the alternate head from XYZ for 99 bucks.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

5

Re: Filament Ratings - Brand / Head Temp / Bed Temp / Type

Fair enough Carl...will edit the post to include Unit Tested

Lightwave 11 / DaVinci 1.0a
www.wditech.com
www.omsmedia.com