Topic: Da Vinci Jr -- major problems
TL;DR: Brand new Da Vinci Jr -- 20 prints attempts and all have failed. Recommend buying the Jr from a place with a good return policy.
Bought the Da Vinci Jr and got it yesterday in the mail from Best Buy. I really wish I had read this forum before buying it (all the official reviews online were extremely positive...). I am using the latest firmware and software. I have not gotten a single print to go longer than 10 seconds without 1) the nozzle making PLA spaghetti or 2) the PLA print coming disconnected from the bed and getting dragged around.
The manual says that the Jr was carefully calibrated at the factory, so I made note that it shipped with a Z-Offset of 1.45 before making any adjustments. I've now tried Z-Offsets of 1.45, 1.55, 1.65, 1.75, 1.85, 1.95, 2.35, etc (printing with and without a raft). I do get the loud banging noise and filament spool shake that others are getting when I print, although I think that subsided when I jacked up the Z-Offset to something ridiculous like 2.5mm. Nothing works and it appears that the Jr doesn't have much more to tweak beyond changing the Z-Offset. The bed itself seems fairly level and I haven't seen the nozzle impact the masking tape.
I have cleaned the nozzle several times with the thin wire pick that the Jr ships with and when doing a "Load Filament" operation, I can get filament to stream out of the nozzle. I've been using the square masking tape-like stuff that the Jr shipped with on top of the glass bed. I also just tried putting blue 3M painter's tape on the print bed instead -- same result.
Unless there is something else I can try, the Jr is getting dropped off at Best Buy (I think I have 15 days to return it) and i'll either try another Jr or just splurge for a Robo3D or Printrbot Metal (which are almost twice the price of the Jr).