Topic: If you have bed adhering issues
I've been having adheing issues especially on bigger prints that would get unstuck. I tried different hair sprays and glue sticks, some performed better than others but still had issues and lots of reprints.
Finally tried 3DLAC and that works amazingly well. Just finished a HTC phone case. A print that I never got to go more than half way before it came unstuck. With this spray, after the print, I tried pulling the printed case of the glass but that thing was not moving an inch.
Let the bed cool and it came off without much force.
Thought I'd mention it as haven't seen any posts about it here.
This is what it looks like (I didn't buy it in that shop)
http://revolution3dprinters.com/shop-pr … ials-3dlac
I can only recommend ![]()