Topic: DaVinci Junior and other software
Has anyone tried other software with the DaVinci Junior, other than XYZware? Things like Octoprint or Repetier for example?
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → XYZ Printing DaVinci → DaVinci Junior and other software
Has anyone tried other software with the DaVinci Junior, other than XYZware? Things like Octoprint or Repetier for example?
Subscribed for interest!
It doesn't look like many people have tried yet with the Junior, but then again it was only released fairly recently.
http://www.soliforum.com/post/115212/
http://www.soliforum.com/topic/12741/xy … nced-mode/
you can slice using a third party slicer, and copy the gcode into advanced xyzware.
as long as you copy the file header from a natively created 3w file you're good to go.
Bringing this back from the dead because I'd love a better slicer but I was told that we can't do anything special with the Jr?
Edit: I'd love to use the advanced version of XYZWare but I have a Mac
I cant change the extruder temp. with xyz advanced.
Can someone help me out?
I cant change the extruder temp. with xyz advanced.
Can someone help me out?
You just have to change one or two lines and uncomment
Change :
23 ; M104 S0 ; set temperature
24 ; M109 S0 ; wait for temperature to be reached
in :
23 M104 S200 ; set temperature 200°C
24 M109 S200 ; wait for temperature to be reached 200°C
And them click on the floppy icon L_SAVE
I'm another Mac user who would like to know if the advanced mode of XYZWare is available and how to activate it.
SoliForum - 3D Printing Community → XYZ Printing DaVinci → DaVinci Junior and other software
Powered by PunBB, supported by Informer Technologies, Inc.