ArcticWolf_11 wrote:what about putting a fan or lowering the extruder temp to 190C would that help? Because its at 200C atm
If you lower the temp or use a fan with ABS that will lead to layer separation and maybe even the part lifting.
We told you what most people who print do to remedy your issue, if for some reason you don't want to follow our advice then you are putting yourself back to the point of when you first asked the question. Because honestly for such a small print there is no alternative. Either print multiples, or print other items of same or taller height so the head can move away from the first model for a few moments.
The only other alternative is to hand edit the gcode and have the head move off to the side for maybe three seconds after each layer is printed. I doubt you want to do as even a small print like this is several thousand lines of code.
Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.