Topic: Prints tend to curl up!
Hello!
I've had my solidoodle press 2 weeks ago and i'm still strying to find the best settings. I would say i'm kinda happy with it ( it's sort of magical when your design emerge from nothing but you know what i mean
).
My biggest problem so far is that when the overhang became intense, the print tend to curl up resulting in my nozzle touching the print and ultimately pushing the part off.
I read manyyyyyyy forum but still don't find a clear answer. Do you have any solution?
Printing setup:
White ABS
Extruder: 250 ( does the same at 210...)
Heated bed: 95