1

Topic: Cura on DaVinci with Repetier limits to 0.2 layer

I installed Repetier on a DaVinci 1.0A and am using Cura slicer. The software only allows me to select 0.2 layer height.
Can anybody explain why it won't offer any other layer heights?
Is there a setting I'm missing?

2

Re: Cura on DaVinci with Repetier limits to 0.2 layer

Welcome Chuck!

I've been holding off on installing Repetier myself. I would be interested in hearing your thoughts about it after you've used it awhile.

Win 8.1
Improved Da Vinci 1.0 with Firmware 1.2.5 and stock extruder
Arduino cartridge resetter and after-market ABS filament
TinkerCAD, Netfabb, Simplify3D

3

Re: Cura on DaVinci with Repetier limits to 0.2 layer

Elproducts wrote:

I installed Repetier on a DaVinci 1.0A and am using Cura slicer. The software only allows me to select 0.2 layer height.
Can anybody explain why it won't offer any other layer heights?
Is there a setting I'm missing?

At the bottom in the Quality window you have to click the +, then you can create a new profile with different layer heights.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

4

Re: Cura on DaVinci with Repetier limits to 0.2 layer

At the bottom in the Quality window you have to click the +, then you can create a new profile with different layer heights.

Couldn't find a Quality Window at first but searched around and then found it under the Slicer tab>Configuration Button then in that menu under the Cura Tab and found the Speed and Quality tab.
Added the different layers and then had to reboot Repetier for them to show up in the object window.

Thanks. Never would have found that without a clue.