wardjr wrote:seven2099 wrote:you dont need to use cura or anything else man. In Soliprint simply select Options->Slic3r options and there you can change all sorts of settings including infill %.
set it to something like 80-90% however don't do 100% because
A) it will be a waste and not actually print as well as 80-90% (since its much much slower)
B) 100% on slicer bugs out
Are you referring to the same Slic3r that many of us use?
The same Slic3r that many successfully print at 100% infill with such great results that we choose to print most things that way?
I have never seen Slic3r "bug out" using 100%.
Your last few posts have been filled with certainty. Yet, that certainty has not been founded in fact. Please help make the forum a better place. If making a "statement of fact" with authority, you'd better make sure you have the facts and are indeed an authority on the subject.
Uh ok. I've submitted a bug report to support for 100% infill in SoliPrint using Slicer via command-line (which is the way soliprint accesses slicer).
In soliprint 1.1.2, using 100% infill and/or scale set to 0, caused a bug in Soliprint (windows only) that caused you get stuck printing the same object permanently since when using 100% infill with the version of Slic3r that came with Soliprint, it would not re-generate valid gcode again.
No re-install of the software, or restart of system, or even of the Press could fix it and it only happened when using 100% in-fill on TWO PCs, on BOTH Presses I've had in my possession. To the bug report I submitted, I also added a work around using the command line for Slic3r to get it semi working agin.
I say it with certainty since, with things types of things that are hard to QA, if a bug happens on 2 printers with 2 different systems running them on windows 8.1 (and not on MacOSX), its probably the fact that, you know, when I wrote the bug I very well knew what the steps to reproduce were since I accidentally ran into the bug on my main PC with my first Press, and then was able to reproduce it with my replacement Press using Soliprint 1.1.2 on a different machine. <- certainty
AFAIK, in the 1.1.4 patchnotes, I didn't read about a fix and my ticket was closed with no feedback despite various people had reported the same issue in windows.
Now I don't print in windows, since my Windows partition doesnt want to print when using SoliPrint.
relax.