Newest XYZware has an option under filament type as flexible. Any one out there have an idea on or if this means a nylon type filament will be available soon?

Thanks

2

Re: XYZware 1.1.35.24

A few weeks ago I saw a box of flexible filament appear under their "filament" options page on the XYZ website. It listed the specs and possible uses etc. It was promptly taken down soon afterwards.

I assume that it will reappear sometime soon. Now, we just need to get it into the stores. The refillable spools have yet to make an appearance and they have been listed for quite some time now.

Win 8.1
Improved Da Vinci 1.0 with Firmware 1.2.5 and stock extruder
Arduino cartridge resetter and after-market ABS filament
TinkerCAD, Netfabb, Simplify3D

3

Re: XYZware 1.1.35.24

PseudoShooter wrote:

A few weeks ago I saw a box of flexible filament appear under their "filament" options page on the XYZ website. It listed the specs and possible uses etc. It was promptly taken down soon afterwards.

I assume that it will reappear sometime soon. Now, we just need to get it into the stores. The refillable spools have yet to make an appearance and they have been listed for quite some time now.


The refills are nothing but spools that come with a chip. You have to crack open one of your old cartridges and swap out the spool and chip in it.

I saw some refills on ebay and amazon just the other day. Microcenter also has had them in stock.