Topic: Buildtak
I have been using buildtak on tha glass bed in my press
and i can only highly recommend it
never need glue spray or abs slurry only need tweek the z offset little lower
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Solidoodle Press → Buildtak
I have been using buildtak on tha glass bed in my press
and i can only highly recommend it
never need glue spray or abs slurry only need tweek the z offset little lower
Did you just got 203 x 203 and stick it directly to build plate? Do you have pictures of your prints on it?
Really? That's cool! Can we see some pictures?
The MakerLab on my campus has Makerbots that use PLA, and they also use BuildTak. I never really thought of using it for ABS, but if it works, I'd be very curious to try it out.
yes i got the one 203 203 works realy great first the z offset was not good enough so i needed lower the z offset
if print 0.1 = z offset 0.09 0.2 = 0.19 0.3 = 0.29 or more just needs little bit more push to the bed then it sticks like glue no warping the only bad thing is if the head crashing into bed then it melts a hole .
i will buy a new one later this one works like a charm