Topic: Accurate sizing - tips to accommodate for shrink/overlap?
Hey all,
I have been doing a lot of small testing with my DaVinci and Im having a difficult time finding the proper sizing method to compensate for ABS shrinking and/or shell overlap. For example, if I model a nut and bolt, I have to upscale the nut in order for it to properly screw onto the bolt.
Im trying to print a ring collar for a 14mm tube with a snug fit. It is proving to be a challenge; either its too large or too small.
My process, so far, has been simple trial and error of printing out a small piece to see how it fits, then adjust the model accordingly.
My test was modeled at 14.77mm and measured with my caliper to be 14.1mm after it cooled, so there is about a .68mm difference.
I cannot tell if the size difference is due to shrinkage or shell overlap.
Is it all trial and error or are there any general tips/tricks to getting the proper sizing tolerance?
Thanks!