Topic: My hot end mods
I made a modification to the stock Da Vinci today and to my surprise
I had to up my extruder temperatures for both PLA and ABS by at least
30 degrees from what I was using for the last month.
I started this project to see if I could make PLA printing a lot
less critical as far as temperature settings and the feed drive
clicking.
Some of you more experienced guys may have gone through this already
but I found its not about adding heat sinks or closing off the air
flow and trying to redirect it or even reversing the fan direction.
It's about more air movement across the upper extruder and heat sink.
I removed the PCB board and mounted off the head assembly.
Half the air flow or more was being blocked off.
I left all of the holes open so air can move more freely and
at a greater volume.
After printing several PLA models and moving the temperature up and
down with reason I could no longer get the feed problem to appear.
I was equally surprised after switching back to ABS that I had to up
my temperature 30 degrees to get the proper flow that I had before.
Time will tell if this modification will prove itself but so far after
several builds in ABS and PLA its working good.