Topic: need help with Makerbor Replicator 2X Custom profile
I am trying to print a Bearing
http://www.thingiverse.com/thing:285779
ABS
no nozzle fan
no raft with support
.2 mm layer height
and the bearings keep coming off the support while printing.
Here is my custom profile
can you tell me what I am setting wrong
{
"comment" : [
"This is a profile for printing ABS on the right extruder with dissolvable",
"support and raft on the left","PURPLE"
],
"version":"3.0.0",
"layerHeight": 0.20,
"layerWidthMaximum": 0.4,
"layerWidthMinimum": 0.4,
"layerWidthRatio": 1.48148,
"bedZOffset": 0.0,
"startX": -110.4,
"startY": -74.0,
"startZ": 0.2,
"defaultExtruder": 0,
"rapidMoveFeedRateXY": 150,
"rapidMoveFeedRateZ": 23,
"minLayerDuration": 5.0,
"minSpeedMultiplier": 0.3,
"doDynamicSpeed": false,
"dynamicSpeedCurvatureThreshold": 15,
"dynamicSpeedDetectionWindow": 3.0,
"dynamicSpeedSlowdownRatio": 0.5,
"doDynamicSpeedGradually": true,
"dynamicSpeedTransitionWindow": 6.0,
"dynamicSpeedTransitionShape": 0.4,
"doDynamicSpeedOutermostShell" : true,
"doDynamicSpeedInteriorShells" : false,
"doSplitLongMoves": true,
"splitMinimumDistance": 0.4,
"extruderTemp0": 230,
"extruderTemp1": 250,
"platformTemp": 110,
"numberOfShells": 2,
"shellsLeakyConnections": false,
"infillShellSpacingMultiplier": 0.7,
"insetDistanceMultiplier": 1.0,
"roofThickness": 0.8,
"roofLayerCount_disabled": 4,
"roofAnchorMargin": 0.4,
"floorThickness": 0.8,
"floorLayerCount_disabled": 4,
"coarseness": 0.0001,
"sparseInfillPattern": "hexagonal",
"infillDensity": 0.1,
"infillOrientationOffset": 0,
"infillOrientationInterval": 90,
"infillOrientationRange": 90,
"gridSpacingMultiplier": 1.0,
"solidFillOrientationOffset" : -45,
"solidFillOrientationInterval": 90,
"solidFillOrientationRange": 90,
"doBacklashCompensation": false,
"backlashEpsilon": 0.05,
"backlashFeedback": 0.9,
"backlashX": 0.0,
"backlashY": 0.09,
"doBridging": true,
"bridgeAnchorMinimumLength": 0.8,
"bridgeAnchorWidth": 0.8,
"bridgeMaximumLength": 80.0,
"bridgeSpacingMultiplier": 1.0,
"doExternalSpurs": true,
"doInternalSpurs": false,
"maxSpurWidth": 0.5,
"minSpurLength": 0.34,
"minSpurWidth": 0.12,
"spurOverlap": 0.001,
"doRaft": false,
"defaultRaftMaterial": 1,
"doMixedRaft": true,
"raftAligned": false,
"raftBaseAngle": 0,
"raftBaseDensity": 0.7,
"raftBaseLayers": 1,
"raftBaseRunGapRatio": 0.8,
"raftBaseRunLength": 15.0,
"raftBaseThickness": 0.3,
"raftBaseWidth": 2.5,
"raftInterfaceAngle": 45,
"raftInterfaceDensity": 0.3,
"raftInterfaceLayers": 1,
"raftInterfaceThickness": 0.27,
"raftInterfaceWidth": 0.4,
"raftModelSpacing": 0,
"raftOutset": 4,
"raftSurfaceAngle": 0,
"raftSurfaceLayers": 2,
"raftSurfaceThickness": 0.20,
"doPurgeWall": true,
"purgeWallModelOffset" : 2.0,
"purgeWallSpacing" : 1.0,
"purgeWallWidth" : 0.5,
"purgeWallBasePatternWidth" : 8.0,
"purgeWallBaseFilamentWidth" : 2.0,
"purgeWallBasePatternLength" : 10.0,
"purgeWallPatternWidth" : 2.0,
"purgeBucketSide" : 4.0,
"purgeWallXLength" : 30,
"anchorWidth": 2.0,
"anchorExtrusionAmount": 5.0,
"anchorExtrusionSpeed": 2.0,
"doSupport": false,
"defaultSupportMaterial": 1,
"doMixedSupport": false,
"doSupportUnderBridges": false,
"supportAligned": false,
"supportLeakyConnections": false,
"supportDensity": 0.35,
"supportExtraDistance": 1.5,
"supportAngle": 10.0,
"supportModelSpacing": 0.15,
"supportExcessive": false,
"doFanCommand": false,
"fanLayer": 1,
"weightedFanCommand": -1,
"doFanModulation": false,
"fanModulationWindow": 0.1,
"fanModulationThreshold": 0.5,
"doPrintProgress": true,
"startGcode": "",
"endGcode": "",
"commentClose": "",
"commentOpen": ";",
"extruderProfiles": [
{
"bridgesExtrusionProfile": "bridges",
"feedDiameter": 1.71,
"feedstockMultiplier": 0.93,
"firstLayerExtrusionProfile": "firstlayer",
"firstLayerRaftExtrusionProfile": "firstlayerraft",
"infillsExtrusionProfile": "infill",
"insetsExtrusionProfile": "insets",
"nozzleDiameter": 0.4,
"outlinesExtrusionProfile": "outlines",
"raftBaseExtrusionProfile": "raftbase",
"restartExtraDistance": 0.0,
"retractDistance": 1.3,
"retractRate": 25,
"toolchangeRetractDistance" : 19.0,
"toolchangeRetractRate" : 6.0,
"toolchangeRestartDistance" : 18.5,
"toolchangeRestartRate" : 6.0
},
{
"bridgesExtrusionProfile": "bridges",
"feedDiameter": 1.73,
"feedstockMultiplier": 0.93,
"firstLayerExtrusionProfile": "firstlayer",
"firstLayerRaftExtrusionProfile": "firstlayerraft",
"infillsExtrusionProfile": "infill",
"insetsExtrusionProfile": "insets",
"nozzleDiameter": 0.4,
"outlinesExtrusionProfile": "outlines",
"raftBaseExtrusionProfile": "raftbase",
"restartExtraDistance": 0.0,
"retractDistance": 1.3,
"retractRate": 25,
"toolchangeRetractDistance" : 19.0,
"toolchangeRetractRate" : 6.0,
"toolchangeRestartDistance" : 18.5,
"toolchangeRestartRate" : 6.0
}
],
"extrusionProfiles": {
"bridges": {
"feedrate": 40,
"temperature_disabled": 230.0
},
"firstlayer": {
"feedrate": 30,
"temperature_disabled": 230.0
},
"firstlayerraft": {
"feedrate": 50,
"temperature_disabled": 230.0
},
"infill": {
"feedrate": 90,
"temperature_disabled": 230.0
},
"insets": {
"feedrate": 90,
"temperature_disabled": 230.0
},
"outlines": {
"feedrate": 40,
"temperature_disabled": 230.0
},
"raftbase": {
"feedrate": 10,
"temperature_disabled": 230.0
}
}
}