Topic: Davinci 1.0 frequent 0010 error
It started occasionally about 2 months ago. Now its happening more frequently.
After a print is finished, and sits idle for few minutes.
A new print job is sent. About 70% into its bed heating the error 0010 will set off.
An on/off power will clear, print job resent and will print.
Anyone have this prob ? Whats the fix ?
Repetier FW 0.92, Solidify3D