Topic: I will test your materials
If you need resin turned into filament and sent back to you (in filament or printed form), I can do that.
Here is an example of an after extrusion review of the resin would look like: http://www.soliforum.com/topic/8528/tpe-versaflex/
PM me for more details. I accept plastics in pellet form, or in solid form (prints or injection molded pieces - I can granulate the plastic)
My Blog http://ggalisky.weebly.com/
My Youtube https://www.youtube.com/channel/UCXShYo … aDUpebDAOw