Topic: XYZ Printing nature ABS
I just checked the product page for the XYZ printing filament on Amazon and found out that they now are offering nature ABS. I am assuming they mean "natural" ABS. I just wanted to inform those who have not seen and have ordered some to see how it prints. Due to the supposed lack of pigment it should in theory have less of a expansion/ shrinkage problem.