Topic: Nothing coming out of the printer head after a few lines
Just got my Da Vinci 1.0 a couple of days ago. I've had some good times with it so far, but have only printed about 4-5 shapes before it stopped working.
The "ink" basically stopped flowing from the printer head. When I remove the filament and reinsert it, I can get about 1 layer at most (fairly big object though) before it stops printing again. Haven't repeated the exercise but I think that little data point is useful for diagnosis. Re-inserting filament gets it to print for a second.
No clicking noise, so I can only assume its being heating properly.
Cleaning out the hole now with the hole cleaner I just found that came with the kit. That had been missing. If this works I'll still post for the community. -- there was some hot glue in there I think. The hole cleaner can't get all the way in there, I assume that's normal. Trying again with sample print:
BY THE WAY. Does anyone else's XYZ Printer software freeze EVERY TIME you print something? I'm using a mac and mine does. god that's incredibly annoying. This software blows. Is there anything else I can use without the sd card hack?
ANYWAY, back to the mission:
"Printer busy" -- the printer is NOT busy. Anyone experience this? The only way I know how to fix this is to get it started with a sample print, then cancel it, then it works again. OH GREAT, now the XYZ printer software froze because I tried to print. NOT PRINTING, because the printer is "busy" or "idle", TOTALLY NOT BUSY. Restarting XYZ software….
Unplugged the USB cable because it thought I had the da vinci 2, reinserted, oh look the printer space got bigger, I guess its working now, great. Derrr it worked that time. God I hate this software. Now we'll see if the print worked….back in a couple of minutes….
Heating up…extruder temp is 213 celcius and unchanging. Platform is 67, just 30 more C to go….
Selah! There was glue stick stuff in the extruder. Think this is solved.
Saving post for future frustrated person(s)
**EDIT: Software frozen now that print is complete. Does anyone know how to fix this??
2nd edit: OK, so its just the print dialog that freezes, the rest of program still works….
update: It didn't work. Only the sample print which was 10mm*10mm*1.5mm worked. Not printing again after less than one layer of successful printing. See below.