Re: Stainless steel and Magnetic PLA filaments
Thanks -- sorry, newbie error, I didn't see that on the site.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → The Latest in 3D Printing → Stainless steel and Magnetic PLA filaments
Thanks -- sorry, newbie error, I didn't see that on the site.
Thanks -- sorry, newbie error, I didn't see that on the site.
no prob. Just wanted to make sure you saw it.
any extruded material is only as strong as the plastic etc that bonds it together. as its just fine dust inbedded into the base material that melts. and yes if the "powdered" material is harder than extruder parts it will be abrasive towards those softer parts just like when using a drill or saw blade on hard materials the blades suffer the end results.
only Laser powder type printers can 'weld' metals etc together. so for the 'desk top 3D printer' industry, these type exotic filaments are mostly for looks with some practical uses for conducting electricity, flexibility, etc. the metals are mostly for costume jewelry and art. but still in demand due to what can be made using 3D tech now.
Got an email mine was shipped today
got mine today and I'm testing with it as we speak. So far 230 c for the hotend and 70 c on a glass bed seems to be right for the stainless steel pla. gunna buff on it in a bit.
Be sure to find a good home for your results in a new thread in the Filaments section of the forum.
Looking forward to your results since I still haven't gotten said email ![]()
Carbon Fiber PLA Specification
Flexural Strength: 57 MPa
Liquefying Temperature: 190°C - 230°C
Elasticity: 45.5MPa
Extension at Break :(73°F) 320%
Standard Tolerance :± 0.05mm
Layer Thickness : 3mm
Shore Hardness :45D
Thickness: 1.3 g/cm3 (1300 kg/m3)
Heat Deflection: 21% to 85°C
Shrinkage: Very Low, When Cooling to Elevated Ambient Temperature
3d printing sevice surat india
Carbon Fiber PLA Specification
Flexural Strength: 57 MPa
Liquefying Temperature: 190°C - 230°C
Elasticity: 45.5MPa
Extension at Break :(73°F) 320%
Standard Tolerance :± 0.05mm
Layer Thickness : 3mm
Shore Hardness :45D
Thickness: 1.3 g/cm3 (1300 kg/m3)
Heat Deflection: 21% to 85°C
Shrinkage: Very Low, When Cooling to Elevated Ambient Temperature
3d printing sevice surat india
SoliForum - 3D Printing Community → The Latest in 3D Printing → Stainless steel and Magnetic PLA filaments