Re: Changing Configuration Issues
I solved this problem, as I mentioned in other threads. The problem was caused by setting the height of the first layer more than the nozzel opening. Thus with a .35 MM nozzle that's the tallest first layer you can use. If you are using the .1MM INI file you can go to that which is triple the normal layer thickness. But, if you are using the .3MM INI file you can only go to .3 or .35MM in first layer height. The error message that shows in the popup says nothing about this. I only discovered it when I happened to look down at the message area of Repetier after it had failed. There it was plain as all get out. Well, it was in a pink and hard to see but there.