Re: ColorFabb Bronzefill
Good luck with the y-axis shifting, you'll solve it.
I find the BronzeFill to ooze when doing large travels across the bed....
I'm about 30 hrs in a 85hr build. I've already burned through a whole spool of the 1500gram and swapped in a second spool. ColorFabb strongly recommends the cooling fan, but I think it varies on hotend and machine... and model sizes too...
My model size: 18.39" x 19" x 8.25" inches...
I think for small sizes, it's a great material, however at large sizes, not so much. As ColorFabb says, it's holds a great deal of heat energy and will have a tendency to sag in Z" (unless quick cooling happens)
I'm experiencing this right now ![]()
From NYC, NY