1

Topic: ABS-T (transparent) for sale.

For those (in europe) who are looking for transparent ABS... look no more, you may buy it here: http://www.dowire.pt

This transparent ABS filament will broad your creative options.  You can now incorporate lights in your 3d objects, creating cool effects, in one go.
It has the same resistance of the opaque ABS but prints with less shrinkage, making it ideal for printing large objects, subjected  mechanical stresses.

http://dowire.pt/image/cache/data/Special%20filaments/ABS-T/175mm_ABS-T-800x640.jpg