elmoret wrote:MINTEMP triggered means its reading less than 5C on the extruder. Can you heat the extruder a bit with a hairdryer, get it to 20C, and try again?
Thanks,
i am going to try that when i am home, i noticed a wire is pulled out at the extruder, must have happened during shipping? it is a small white rubber tube, looks like a speaker wire, but there doesnt seem to be anything inside? There are two small white wires that come out of a small light blue plastic piece, one looks to be either broken or just never put in, the cut seems pretty clean.
my house is set to 17 degrees Celcius i think, and my heating bed flucuates between 16-17.5 degrees? the heating bed will not heat up either.
I tried to navigate through the x,y,and z axis. the only thing it will do is go "home"
any ideas anyone?
thanks