docterhow wrote:Just got it today, and printed the demo. Now when I try to print anything it gives me the error code 0040. I want to know what I can do to get it working again. It is the 1.0 model and had 1 successful print. All 3 samples do not print nor does xyzware without the error code.
The usual cause of this error is that the machine cannot write the file to memory. If you open the door on the lower back of the machine you will see the controller board. On the right edge of that board is an SD card. That is this systems memory and working area. It may not be seated well or could have come loose during transit. The only possible way to make sure is to to take out all the screws holding the main board in and then leaving all the cables connected just pull the board far enough away from the side of the machine so you can pull the SD card out and reinsert it.
However if this is a new machine and under warranty I would contact XYZ for an RMA number and send the unit back for repair or replacement since opening the back and removing the screws on the board may void your warranty. The fault is in the SD card.
Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.