1

Topic: Extrusion speed

I'm sorry if this has been answered somewhere earlier, couldn't really find the SEARCH button neutral

Simple question: how much filament does a Filastruder output in one minute or one hour?

2

Re: Extrusion speed

Search is at the top of the page.

Filastruder specifications are on the product page:

http://www.filastruder.com/products/filastruder-kit

1kg/12 hoyrs, or twice as fast as a typical printer can consume it.

3

Re: Extrusion speed

Doh sorry, I'm used to find it on top right or straight with a field in the forums list.

Thank you for info!