1

Topic: 2 year anniversary of Filastruder - take 15% off until 10/21!

It was this time two years ago that I first had the idea for what would become the Filastruder, and I wanted to say thanks especially to those of you that have supported the project here on the forums.

As a result, you can take 15% off all purchases now through Monday night with coupon code 15off. This is a great time to pick up any accessories you may have been eyeing, or a second Filastruder to run a second material without switching back and forth.

http://www.filastruder.com

After Monday, you can use coupon code 10off for 10% off the rest of the week.

Happy 'struding!

2

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

Dang, and I just ordered and entire package.  I guess the early bird chocked on the worm this time. smile

If you build it they will come. Then they will make fun of it, tell you it's not worth doing and go home and try to copy you.
If a picture is worth a thousand words then being there is worth a thousand pictures.

(2) Stock Makerbot Z18s, Filastruder w/Melt Filter, Filawinder, Autodesk Inventor Design Suite 2014 .........so far.

3

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

Credited you the difference. smile

4

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

You guys are the BOMB!  And to think I was just making a joke.

If you build it they will come. Then they will make fun of it, tell you it's not worth doing and go home and try to copy you.
If a picture is worth a thousand words then being there is worth a thousand pictures.

(2) Stock Makerbot Z18s, Filastruder w/Melt Filter, Filawinder, Autodesk Inventor Design Suite 2014 .........so far.

5

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

...and I still have nowhere to place a Filastruder.
This makes me cry sad

Printit Mason and Printit Horizon printers
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

6 (edited by Superdave 2014-10-19 23:34:42)

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

Azerate,

Come on.... dining rooms are so overrated. big_smile

If you build it they will come. Then they will make fun of it, tell you it's not worth doing and go home and try to copy you.
If a picture is worth a thousand words then being there is worth a thousand pictures.

(2) Stock Makerbot Z18s, Filastruder w/Melt Filter, Filawinder, Autodesk Inventor Design Suite 2014 .........so far.

7

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

Got a question about pellets. In theory a pound of pellets produces a pound of filament?

SD3, E3D hotend,linear bearing on x/y axis',pillow block bearing on y conneting rod, ball bearngs on front y axis, fan on y stepper motor.

8

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

In both theory and application, yes. Mass out is equal to mass in.

9

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

elmoret wrote:

Credited you the difference. smile

More than customer service.

Ulitmaker 2, a few repraps, Custom Big FFF 3D printer with heated chamber.

My Blog http://ggalisky.weebly.com/
My Youtube https://www.youtube.com/channel/UCXShYo … aDUpebDAOw

10

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

one for abs one for pla woot woot

11

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

Darn, I wish I found the filastruder 3 months ago.

12

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

Are there any coupons running right now?

SD Press - v1 (Pre-order) / RAMPs /w DRV8825's / Cyclops (25w) / Dual Bowden / Mk8 Gear / MK2b PCB Heat bed /w custom replacement Z / PEI Bed
SD2 / E3D v6 / Direct Drive / Mk8 Gear / RAMBo v1.3 / PEI Bed / Anti Z backlash mod / Ikea Expedite enclosure.
Both Driven by Octoprint (devel) via a RPi B+ / Neopixel status alerts / GPIO Controlled SSR / (SD2) 450 Watt PSU for remote power-up/shutdown.

13

Re: 2 year anniversary of Filastruder - take 15% off until 10/21!

'reprap' for 5% off an e3dv6.