Topic: printed a "Google Cardboard" viewer with DaVinci
Fooling around with a Google Cardboard VR viewer that you can purchase on Amazon for $9 but found the cardboard is a bit flimsy and gets dirty pretty fast. Search and found a Google Cardboard for Samsung S5 on Thingiverse that works very well. The 3D print on the Da Vinci 1.0 had all holes too small and needed some work to make them fit. The worst hole was where the lenses are supposed to sit. Otherwise, it works as advertised. -- ggunners
XYZ DaVinci 1.0 stock ABS, Simplify3D
QUBD Two-Up PLA, new 3D printed X gantry, Y idler, flex z coupler, extruder mount, E3D Lite