Here at ridix.nl we tested the lowest printing resolution with home acetone treatment.
This way we can find out to what degree acetone really changes the surface.
As you can see, the result is way smoother after the acetone treatment.
I'm sure someone else also pointed this out in the past, but some other beginners in de 3D printing world might not know this little trick. Do you have any other surface treatment tricks for these people as well?
Ralph.