Hello,
I've just changed to slic3r, with the recent .ini published from solidoodle.
Trying just .3mm now, but I don't know how to solve this:
This is a 20mm cube. No raft. 95º base and 195º print. I've tried 200 and 205 and base 90 to 100. Same results.
I've calibrated the amount of filament and the flow rate. Very accurate after first millimeters.
But the first millimeters doesn't have the right measure. I've attached a photo and a image to show it better.
It sticks great to the base but It deforms the size of the first millimeters...
So, tested different temperatures, changed first layer to 150% and 200%... Doesn't solve this.