Re: Part not sticking in corners when printing at .1
Interesting results.
Had alot of strings to clean up under the chin and ears.
The main thing is that just above the eyes the layers shifted over about 4 perimeters, kept printing up about another 25 layers then shifted over again. I have seen this before and have never been able to explain it.
I believe the motors get really hot on a good day, so a 27 hour print on a really hot day I think has caused the motors to miss align or something like that, it is uniform around the part so it wasnt caused by the print shifting on the bed or anything.
Pictures attached, only taken with an iphone..believe it or not I actually I dont own a digital camera...weird.