1

Topic: REV E - what should be the right reading?

Hi Guys,

I am testing my drivers in my solidoodle 2. I have the REV E version that has built in drivers.  I am confused which one to follow.. solidoodle wiki or solidoodle support? at wiki the E should be .770v... at solidoodle support website it should be .250V?

2

Re: REV E - what should be the right reading?

well i guess I needed .80v for the extruder to make it work perfectly. .250v is way low