Topic: warping problem even with heated bed?
Okay so I've set my bed temp to 110C in Repetier and head temp to 215. Using Solidoodle ABS filament. I printed few test prints and there's a warping problem. Also I have to set the gap between the head and bed really small and caused the first layer to really smear otherwise the first layer doesnt stick to the heated bed.
What can be the problem? Has the recommended bed or extruder head temperature gone even higher with latest SD4? Or is the problem something else?
Here's a photo of how bad the warping is. It's actually so bad the object unstickied and the print head started moving it with it.

The stl of the print: http://www.solidoodles.com/uploads/doodle?id=424
Especially on the bottom right you can also notice how smeared the first layer had to be.