Topic: Nut & Bolt...
Anyone tried printing a nut and bolt and seeing if they screw together?
always wondered if they would...
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Solidoodle Discussion → Nut & Bolt...
Anyone tried printing a nut and bolt and seeing if they screw together?
always wondered if they would...
I did this a few nights ago, its a snug fit but they twist fine. ![]()
Hi,
Some you can find here: http://www.thingiverse.com/search?q=Thr … ;sa=Search
Regards, wolfi
cheers brad,
all good wolfi, i run keycreator...i just input what thread i want on what sort of bolt and it spits out a solid model i can use.
I had to scale the nut by 1.05 or something to make it fit my bolt. Otherwise it didnt fit.. Havent done many tests and configurations though.