I have been having some pretty weird problems since getting RH v1.0.2.
1: I can print well for a few days then out of the blue my extruder temp fluctuates wildly. The temp is set at 210 but it goes up to 230+ at times then does nose dive and won't recover. I have tried reinstalling, and turning off and restarting.
2: after slicing and temps say they are good it has started to show a dry run in the at a very rapid pace. I have made sure that I did not have dry run selected.
Solidoodle 2 with J-head hot end otherwise stock
SainSmart 1.75 ABS
Heated bed with mirror with hairspray