Topic: tooth character
so we were ask to print this character tooth for a local dentist, as reference i was given a single picture. so i give it a try in zbrush and it came just fine... not so much the first 3d print... i try to separate the "hair" from the body but it just complicated things... not to mention the wasted material trying to make it a solid piece... at the end 30%filll on PLA slow 3mm print came out just fine... for the mouth i ruin several pieces trying to print the curve shape with supports... all came looking messy because of the extra material... finally ... i decided to print the mouth flat and use a heat gun(?)pistol(?) and slowly bend the mouth in the the body shape...finally some crazy glue for mouth and finish!.... has anyone has oven their pieces to give it a shiny look? i tried this with the heat gun and got some nice result....i may oven the left over pieces to see what i can get....
thanks for any comment and tips...
cheers!!!