Topic: Filament Problems
Any one else have this problem. So I ran out of black ABS, right as I was on the last part, Dang!
So I ordered some more black ABS, but not the cartridge type, a 1kg spoil of Black abs. So got it popped it in the printer and I had a problem with it coming out to slow, so it made all of the prints flimsy and can break in your hand. So I though it maybe the reset EEPROM that I had in it because it was for white. So I took it out and put in the old black cartridge and did a small test print and it worked fine. But there was only 8m left on that chip so I reset it with bed temp 90C and extruder 210C. And now I have the problem again. I also reset it to 230C, still the same problem. Any idea?
Does and one know the EEPROM setting for the Arduino code for different extruder temps?
I know 210C is char et[] = {0xd2,0x00}; // 210 C
And 230C is char et[] = {0xe6,0x00}; // 230 C
I don't know EEPROM coding all that well.
Thanks Every one