Topic: Reclaiming t-glase?
http://taulman3d.com/t-glase-features.html
Environmental - While t-glase is not biodegradable like PLA, it is a material that’s considered 100% reclaimable. Thus the new “struders” that convert failed prints back to usable line work perfectly with t-glase. If you have a “struder”, you can actually mix in 12% of the total weight in discarded clear water bottles. Please keep in mind, that the polymer used in most water bottles, has a slightly higher melt temp and that adding them to the mix, may increase print temp a few degrees.
Anyone try this?
Filastruder
NYLON (taulman): http://www.soliforum.com/topic/466/nylon/