1

Topic: Slic3r 0.9.9 fills holes and 1.0.0RC2 makes them...

I've created a model in Sketch Up and exported it as an STL file but when I go to slice it using the stock Repetier/Slic3r it complains there are holes in the model and fills in the slots improperly. I've checked the model for holes, inverted faces and intersecting face but I can't find any. I also tried to fix the model with Netfab but got the same results.

After that tried updating to the most recent version of Slic3r and it no longer complains about holes and after slicing shows the slots properly but leaves sections of the model unfilled with the infill exposed.

I've attached the STL file I'm using along with the model in the preview window (03a), the Slic3r 0.9.9 output (04a), and 2 images of the output of the same file from 1.0.0RC2 (01a & 02a).

Let me know if there are any settings you would like to see and I'll post them. Any help would be greatly appreciated.

Post's attachments

01a.jpg
01a.jpg 62.67 kb, file has never been downloaded. 

02a.jpg
02a.jpg 60.8 kb, file has never been downloaded. 

03a.jpg 44.09 kb, file has never been downloaded. 

04a.jpg
04a.jpg 58.36 kb, file has never been downloaded. 

Base-210untitled.stl 293.52 kb, 7 downloads since 2014-05-09 

You don't have the permssions to download the attachments of this post.

2

Re: Slic3r 0.9.9 fills holes and 1.0.0RC2 makes them...

Slic3r 1.0.0RC3 Sliced it just fine but you need to have the infill set to 1 (100%).  I would bet that to be the case for any of the versions though.
Hope that helps.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

3

Re: Slic3r 0.9.9 fills holes and 1.0.0RC2 makes them...

Could you tell me where this setting is? I've attached photos of the infill settings tab on both and I don't see the setting your referring to.

Also, I've attached photos of the result of printing the part with the hole as shown in the photo. Strangely, if I rotate the part on the table the layers it doesn't fill correctly change and I've been able to print some versions of this model that still have the problem (but not on any of the top or bottom layers where it would be seen) by printing them on a slight angle, but I'd really like to know what I'm doing wrong to cause this...

Post's attachments

099-infill.jpg 100.3 kb, file has never been downloaded. 

100-infill.jpg
100-infill.jpg 102.89 kb, file has never been downloaded. 

P1010172a.jpg
P1010172a.jpg 473.01 kb, file has never been downloaded. 

P1010173a.jpg
P1010173a.jpg 567.46 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

4

Re: Slic3r 0.9.9 fills holes and 1.0.0RC2 makes them...

The first line reads "Fill density"  Change that to 1 and that is 100% you currently have it set to .3 or 30%.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

5

Re: Slic3r 0.9.9 fills holes and 1.0.0RC2 makes them...

I still get the same result but every layer that was crossed hatched is now solid. There are still holes left in the same places.

6

Re: Slic3r 0.9.9 fills holes and 1.0.0RC2 makes them...

I can't attach the g-code file because the forum server said the file was to large so I sent you an email.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions