Topic: Filastruder running very slow.
Thanks for all the help so far. I finished my Filastruder the other day and when I started my first batch it took 8 hours to get half a pound done comes out to be less then 6 inches a second. Is this normal? Will it speed up eventually after a couple runs. Ive been running it with the abs at 180 Celsius the stuff that it comes with. Thanks again